Introduction

logo of solid solution strengthened alloy

Solid Solution
Strengthened Alloy

Iron
Nickel
Chromium
Corrosion
Resistance
77
Mechanical
Behavior
69
Purity
85

Corrosion Resistance

Sulfuric
Acid

Hydrochloric
Acid

Hydrofluoric
Acid

Phosphoric
Acid

Nitric
Acid

Organic
Acids

Alkalies
and Salts

Seawater

Overview

As a leading supplier & manufacturer in India, RAHUL FERROMETAL supply cost-effective Incoloy 864 Products.

INCOLOY® alloy 864 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, thermal stability and resistance to hot salt corrosion, pitting and chloride stresscorrosion cracking. INCOLOY alloy 864 is covered by U.S. Patent 5,827,377.

Corrosion Resistance

INCOLOY alloy 864 was first developed as a corrosion-resistant material specifically for automotive exhaust systems. Most of the data presented in the following pages relate to that area of application. However, the alloy’s potential for other, non-automotive, applications is of sufficient interest to pursue laboratory test programs in other media. Iso-corrosion charts for INCOLOY alloy 864 in hydrochloric and sulfuric acids are presented at the end of this section.

Main Standards

ASTM A240
Sheet and Strip
ASTM A480
Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 8.02
lb/in.3 0.290
Melting Range °F 2467 - 2539
°C 1353 - 1393
Permeability at 200 oersted (15.9 kA/m) 1.004
Electrical Resistivity at 70°F (21°C) ohm•circ mil/ft 628
μΩ•m 1.04

Mechanical Properties

Test Temperature Hardness Tensile Strength Yield Strength Elongation Fracture Location
Rb ksi MPa ksi MPa %
70°F (20°C) 82 79.9 550.9 46.1 317.9 17.4 Weld
70°F (20°C) 83 80.4 554.4 45.3 312.3 18.7 Weld
800°F (427°C) N/A 64.5 444.7 31.7 218.6 20.5 Weld
1000°F (538°C) N/A 58.4 402.7 30.9 213.1 16.6 Weld
1200°F (648°C) N/A 58.9 406.1 28.9 199.3 18.4 Weld
1400°F (759°C) N/A 40.9 282.0 26.4 182.0 23.5 Weld
1600°F (871°C) N/A 23.4 161.3 15.9 109.6 55.0 Weld
More +
More +