MONEL
INCONEL
logo of RAHUL FERROMETAL
INCOLOY
HASTELLOY
Top Hastelloy Alloy G-3 Wire Rod Manufacturer / Supplier in India

Hastelloy Alloy G-3 (UNS N06985)Wire Rod

  1. HOME
  2. Hastelloy Alloy G-3 Wires
  3. Wire Rod
 India Hastelloy G-3 wire rod supplier Indian Hastelloy G-3 wire rod manufacturer Hastelloy G-3 wire rod stock in  India Hastelloy G-3 wire rod from big mill  India Get factory price for sale from Hastelloy G-3 wire rod manufacturer  RAHUL FERROMETAL
 India Hastelloy G-3 wire rod supplier Indian Hastelloy G-3 wire rod manufacturer Hastelloy G-3 wire rod stock in  India Hastelloy G-3 wire rod from big mill  India Get factory price for sale from Hastelloy G-3 wire rod manufacturer  RAHUL FERROMETAL

Hastelloy G-3 Wire Rod Supplier

As a Indian leading Hastelloy materials supplier, RAHUL FERROMETAL produces and manufactures cost-effective Hastelloy G-3 wire rod.

HASTELLOY alloy G-3 (UNS N06985 / W.Nr. 2.4619) is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to yield increased resistance to heataffected-zone (HAZ) corrosion and improved weldability. Alloy G-3 has excellent corrosion resistance to oxidizing chemicals and atmospheres.

Hastelloy G-3 wire rod is a coiled Hastelloy G-3 rod, which is continuously hot rolled from a Hastelloy G-3 ingot. The Hastelloy G-3 wire rod produced by RAHUL FERROMETAL has outstanding corrosion resistance and high temperature resistance, excellent roundness and white surface. Hastelloy G-3 wire rod also has good flexibility and workability, so it is also the raw material for our various Hastelloy G-3 wires. We produce high-quality Hastelloy G-3 wire rod in strict accordance with ISO 9001 standards.

Customized Dimensions

Diameter (D)
6.0 ~ 20.0
mm

High precision Tolerance Available

*Customized size please confirm with us

Standards for Hastelloy G-3 Wire Rod

ASTM B581
ASTM B472
ASME SB 581

*As a professional manufacturer, our default standard for Hastelloy G-3 wire rod is ASTM B581. We can also produce according to other standards as per you required.

Surface to be Customized

Photo of pickled wire rod
Pickled Surface
Photo of bright wire rod
Bright Surface

Chemical Composition of Hastelloy G-3

*Chemical Composition According to ASTM B581

Data Sheet

Physical Properties

Density g/cm3 8.14
lb/in.3 0.294

Mechanical Properties

Condition & Size Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
MPa, min MPa, min %, min %, min Rockwell, max
N06985 / 7.9mm to 19.05mm, incl 621 241 45 ... ...
N06985 / Over 19.05mm to 88.9mm, incl 586 207 35 ... ...

*Mechanical Properties According to ASTM B581

Hastelloy G-3 Applications

Other Informations

Package

thick woven plastic bag

Plastic Bag

wood reel

Wood Reel

wooden case

Wooden Case

Logistics

a logo of steamship

By Sea

a logo of aeroplane

By Air

Price Term

FOB
FCA
FAS
CFR
CIF
CPT
CIP
DDU
DDP
DAF
DES
DEQ
EXW